Fasteners and Finishes

By Thomas S. Doppke
Technical Presentations Co.
Sterling Heights, Michigan


visit the complete series of Fasteners and Finishes.

Part I, Part III, Part IV
Part V, Part VI, Part VII.
Plating Zone

Print this article

Part II

When a bolt is tightened into amating threaded part, the two components interact by pulling each other together. This force is called clamp load and is what keeps thejoint from coming apart. Provided that the force pulling it together is greater than the outside forces (service loads) that are trying to pull it apart, no problem will result with the attachment. Unfortunately, friction plays a large part in this system. Of 100 pct of the torque applied to fasteners to pull them together, 50 pct is lost in underhead bearing face friction and 40 pct is lost through friction between the mating threads. This leaves about 10 pct of the torque applied to actually pull the parts up to the required clamp load. The fastener's finish has a greater influence on tension than any other factor. Depending upon the coefficient of friction of the finish on the fastener, clamp load differences of more than 150 pct are possible on the same part. As Figure I (below) shows, a decrease of 10 pct in friction would decrease the underhead friction about five pct and the thread friction about two pct. While this does not seem like much, the decrease adds 70 pct more to the clamp load required.

The addition of a lubricant or oil to a coating to improve the fastener's corrosion resistance also lowers thread and bearing face friction. This is the most common unauthorized addition. Usually it is done by a verbal request from the customer's assembly plant (and without the engineering department's knowledge), because the assembly line feels that the parts are too dry, rough or hard to assemble.

Graph
WHAT HAPPENS to input torque when friction is decreased.

In the modern and complex world of fasteners, the customer will often not know just what coating or finish he needs for a part and will solicit information from the finishing source. One of the first questions that should be asked is, "What is the intended end use for this part?" Critical attachments (brakes, steering, suspension) require that the customer have some actual joint testing performed and know what finish was on the validated parts. The finish should not be changed without re-validation. Non-critical attachments could be left to the finisher's experience, cost considerations or other factors besides torque-tension relationships. Generally, electroplated finishes with minimum salt spray hours are fine for non-critical areas and areas not subjected to cut extremes. Many of the new dip/spin organics offer high hours to corrosion failure but fill up threads and cause gauging problems. Their thickly deposited coatings interfere with torque tension as well. However, many do have low coefficients of friction and are usable with proper testing on undersized parts.

Changing finishes and topcoats can cause major havoc during assembly when different friction forces interact. It is best to make no substitutions, additions or omissions without documentation to and from the customer that such a modification has been made and is acceptable. In cases where someone other than the original purchasing customer calls and directs modifications, a quick call to the customer's engineering department to confirm the request can save a potential headache. PF