[ Article Archive | or use your back button ]

Chemical Switch Cuts Costs, Improves Safety

By replacing the sodium sulfide chemistry used in its nitrogen oxide (NOx) scrubber with a non-hazardous NOx control chemistry, ChemResearch Co. Inc. (CRC; Phoenix, AZ) reduced its operating costs and eliminated a health and safety hazard.

Jennifer M. Kirtland


Scrubber Technology: An Update
This article discusses changing the chemistry in
a packed-bed scrubber. If you want to learn more about trends, systems and maintenance of scrubbers, read this article.

get info

...Visit Bionomic Industries Inc.'s PF Online Showroom, call 201-529-1094, or select the Product icon on the right.

Cleaning/Pretreatment Zone
print this article

The BIONOxSOLVER™ chemistry, developed by Bionomic Industries Inc. (Mahwah, NJ), provides CRC with a safe, easy-to-handle, high-efficiency NOx scrubbing solution that eliminates the production of toxic and odoriferous hydrogen sulfide gas.

bottom section of the scrubber
The bottom section of the scrubber shown in with
tote container of BIONOxSOLVER.

Since 1998, CRC had used sodium sulfide chemistry in the NOx scrubber at the end of its dedicated aluminum precleaning process. Used to prepare a cast aluminum cylinder for a small engine for hard chromium plating, the automated line cleans and etches the parts using various cleaner and acid baths. The acid baths contain nitric/water or straight nitric/hydrofluoric mixtures. Each load of parts has about 450 sq ft of surface area, with one load processed every seven to eight minutes, sometimes around the clock. When the parts come out of the acid baths, a large volume of NOx is released.

Captured by a ventilation system, the acid fumes are taken to a dedicated 10,000-cfm vertical packed-bed NOx scrubber. “A number of factors led us to begin looking for a less labor intensive and less hazardous alternative to the sodium sulfide chemistry,” explains CRC Director of Regulatory Affairs and Facility Development David Weed. “Making up that sodium sulfide tank was time-consuming and generated potentially hazardous vapors. Since the chemistry was potentially subject to annual regulatory reporting requirements, we were required to perform and maintain time-consuming record keeping.”

feed line going to the scrubber
The feed line going to the scrubber and top of the tote of BIONOxSOLVER.

According to Weed, sodium sulfide use, coupled with sodium hydroxide, generates scale buildup on the scrubber tank and packing, making cleaning and maintaining the system labor-intensive. The scrubber also required an annual cleaning, which took approximately 28 man-hours, as well as the purchase and disposal of five drums of hydrochloric acid.

About the Company

ChemResearch Co. Inc.
1101 West Hilton
Phoenix, AZ. 85007
Phone: (602) 253-4175
FAX: (602) 254-0428
E-Mail: Info@chemresearchco.com

ChemResearch Co., Inc. is a multifaceted plating, anodize and grinding facility. It serves the needs of the aerospace, electronic, commercial, automotive and medical markets both local and national. It provides services in the areas of Hard (Type III), Sulfuric (Type II), Chromic (Type I) Anodize, Chem Film (Conversion Coat-Irridite), Electroless Nickel (Both Mid & High Phos.), Copper, Nickel, Dry Film Lubricant, Paint, Zinc Phosphate, Silver, Passivate, Internal (ID), External (OD) and Centerless Grinding.

CRC was also concerned about the safety of the tank itself. It was inside another lined tank, vented with an exhaust duct into the scrubber to prevent release of fumes into the atmosphere and in a secure fenced area surrounded by a containment curb. But a heavily used railroad track was just feet away and a derailment could pose an extreme hazard.

Scrubber with a tote container
Scrubber with a tote container of BIONOxSOLVER.

Weed learned that BIONOxSOLVER could potentially alleviate all these concerns, and decided to try a trial conversion. Because the product is delivered in ready-to-use totes, CRC personnel don’t handle it. Instead, a worker moves a tote into place and inserts a pickup tube from a metering pump. “With the sodium sulfide chemistry, we had to fill the tank with water and use a mixer motor to dissolve the sodium sulfide flake,” Weed recalls. “This was a very undesirable task, especially during the summer here in Phoenix.”

As a result of the chemical switch, CRC has reduced its labor costs by about 75% by eliminating many of the procedures the former chemistry required. The scrubber is easier to maintain and there is little to no scale buildup. Annual cleaning, required with the sodium sulfide chemistry, has been eliminated.

The company gained additional savings by eliminating protective gloves, aprons, respirators and cartridges required for handling sodium sulfide. Because the new chemistry does not require the 19,000 gallons of water and the electricity for the mixer motor that the sodium sulfide solution needed annually, CRC is saving another $450. The pH operating range was also reduced from prior levels, cutting the amount of caustic used and purchased.

“Converting to the new chemistry was completed in a weekend,” Weed says. “As a result of the conversion’s ability to help us reduce an on site hazardous material, we accomplished a pollution prevention goal that we set with our state EPA office.” The new chemistry also virtually eliminated health and safety risks to employees, he added.



Zones | Suppliers | Products | Articles | Events | Clinics | Subscribe | Advertise | Contact Us

Products Finishing Magazine. The Definitive Web Resource For Product Finishing Professionals
®2010 Gardner Publications, Inc.