[ Article Archive | or use your back button ]

Electronics Evolution

Plater adjusts operations to meet changing customer demands

By Jim Destefani, Editor


Oscar Unveiled
Precision Plating performs precious metal plating processes mainly for electronics applications.

get info

...about powder coatings, visit Precision Plating Co.'s PF Online Showroom, or select the Product icon on the right.

powder coating zone
print this article

Precision Plating Company (Chicago) knows more about change than many companies.

Launched in 1904 as a decorative plater for production of picture frames and other religious artifact items sold by Chicago’s Marshall Field & Co. department store, the company continued mainly decorative work for the first few decades of its existence.

That began to change in the 1930s when the military approved Precision as a supplier. Then, in the 1970s, the owners hired Jim Belmonti to set up the company’s new plant. Belmonti intensified the company’s focus on the burgeoning electronics plating business, which remains Precision’s main application area today.

Through the 1970s and ‘80s, Precision grew by staying abreast of electronics industry trends and developing and using some proprietary processes in-house. An example is the company’s soffering of palladium-nickel as an alternative to gold plating during a time of extremely high gold prices. After years of persistence by Jim Belmonti working with AT&T Bell Labs, IBM eventually agreed to use the material for connectors in its new System 2 computer. The first year, Precision plated 1.4 billion contacts.

By 1989, when the then-owners were looking to sell and retire, Jim Belmonti made an offer to purchase Precision. The company is currently managed by the second generation of Belmontis and the team built by Jim.

manual barrel and rack plating lines
Small, manual barrel and rack plating lines make up one of the main components of Precision’s capabilities. Process upgrades focus on increasing flexibility for variable lot sizes.

According to Jeff Belmonti, the company’s culture and passion for the plating business are clearly intact from Jim Belmonti to the new generation. “My father had worked for other plating companies and suppliers of plating chemistry,” Jeff Belmonti says. “He went into a lot of dark, dirty plating shops, and as a result he wanted to have—as he put it—a plating shop where a woman could wear high heels: well-lit, clean, no water on the floor.”

Jim Belmonti’s contributions to Precision are also seen in the reel-to-reel portion of the business in the form of several selective plating methods brought to fruition under his leadership. Stripe-on-strip plating is another technique Precision mastered in the 1980s, when pagers were at the height of their popularity.

Although popular electronics have changed, Precision has carried on this approach to its business. The company continued to grow. Eventually, its stable of processes grew well beyond rack and barrel with reel-to-reel plating of copper; multiple silver, gold and other precious metal processes; electrolytic and electroless nickel; and several types of tin plating.

Lean Thinking
More recently, lean manufacturing concepts such as minimizing work-in-process and just-in-time delivery have increased in popularity among manufacturers in some segments of the electronics industry. This is the latest trend that has Precision making adjustments to the way it does business.

Small lots and quick turnarounds
Small lots and quick turnarounds are the norm in the company’s reel-to-reel and stripe-on-stripe plating area. Metals plated using these processes include nickel, gold, silver and palladium.

“Just-in-time, lean manufacturing, whatever you want to call it, has impacted business in a big way,” says Jeff Belmonti. “If a customer needs to build 250 of something that requires a plated component, they send us 252 pieces and we turn the order around overnight. Our reel-to-reel area works that way as well—a lot of small-volume, quick-turnaround jobs.”
Offshoring, and global political and economic events, are also impacting Precision’s business. “NAFTA has helped us a lot, because a lot of our stuff goes to be assembled in plants in Mexico or Canada,” Jeff Belmonti says. “The weak dollar helps, too.”

Jeff’s brother Gary Belmonti explains how the globalization of electronics manufacturing has been both a blessing and a curse for Precision: “What our customers figured out is, it’s better to have five manufacturing plants in different parts of the world than it is to have one big plant. So they still have a plant, for example, in Illinois to cover the U.S. and Canada. They may have a plant in Mexico and a plant in Asia. So that creates opportunities. The difficult part is keeping track of all the players and keeping tabs on potential jobs that are being tooled for production in the US market.”

Precision Plating is developing methods to address customers’ demands for fast turnarounds in ways that make sense economically. “Our big focus in the last year is meeting a guaranteed promise date,” Jeff Belmonti says, “and we are implementing production techniques to meet request dates.”

Shop-Floor Changes
Out on the floor, the switch to low-volume, just-in-time production is translating to multiple capital improvement projects on both the rack/barrel and reel-to-reel sides of Precision’s business.

Display in a centralized control room
Display in a centralized control room provides an overview of the facility’s waste treatment system.

“On our barrel lines, we’re trying to make the shift from manual to automatic operation,” explains Erik Probasco, general manager of rack and barrel operations. “The problem is, historically, automatics require huge batches of parts to make sense. That’s not the way things operate any more. So we’re trying to get to where we can actually take 12 pieces, 80 pieces and 10,000 pieces, load each unique process at the same time, and run them simultaneously.

“Flexibility and efficiency need to be built in together,” Probasco continues. “We know that the processes we perform are not going to change much over the next few years, but how we’re going to get the work out is going to change. So it’s not about building a line for a single customer part program that you have to run, it’s about building a line that can run five or more programs.”

Proprietary Processes at Precision
Development and use of proprietary processes has played a role in Precision Plating’s growth since the 1970s. Here’s a quick look at some of the processes pioneered and used by the company.

Brush microplating uses an absorbent medium, such as felt, to apply the process solution on the part area being plated. The medium may be in the form of a roller or another configuration that conforms to the contact form. The medium is saturated as it turns through the plating solution, allowing the solution to plate only in the area making contact with the roller. Brush plating is a good way to limit plating to the raised contacting surfaces of electrical contacts, and can even be employed to plate only one or two sides of rectangular connector pins. Precision used the process in the early 1980s to reduce gold consumption 87% at a time when gold prices were extremely high.

Reel-to-reel plating generally consists of stamped configurations, carrier-held bandolier or flat stock to be plated for forming later. Applications are in the connector, computer, automotive and consumer appliance industries.

Stripe on strip is a variant of reel-to-reel plating that is used to apply a “stripe” of precious or non-precious metal plating to solid flat stock. After stripes are applied to tight dimensional tolerances, the flat stock can be run through a stamping press. The process allows stampers to process pre-plated material that has plating only in the areas required for the final part configuration.

Stripe-on-strip technology was integral to various electronics industries advances, particularly the pager. It made possible major cost savings to both electronics manufacturers and consumers. Precision worked very closely with customer engineering groups to integrate this technology into their products.

An example of the emphasis on improved flexibility is a project to refurbish one of Precision’s automatic rack lines. “We got rid of the PLC that used to control the pumps and rectifiers,” Probasco says. “We still have a PLC to control the hoists, but everything else—temperature controls, rectifier controls—is separate. With this approach, if we want to change any process parameter we can easily do it.”

A brand-new barrel line is also aimed at fast-turnaround, small-lot production of precision parts. The new line will include a cleaning cycle, cyanide copper underplate, sulfamate nickel, bright and matte silver, and hard and soft gold processes. “It’s really a small offshoot of our precious metal line, and we will be doing this for non-precious metal processes, too,” Probasco explains.

The line includes a hoist in case it’s needed for heavier components, but it is tailored to provide quality and control for small load sizes, according to Probasco. “Tanks, rectifiers, all the equipment is sized for small lots,” he says. “We kept the tanks as small as we could. The rinsing method we chose—a triple counterflow rinse made for barrel plating—will help us get good rinsing while minimizing water usage. The first rinse is a spray that goes to drain. The next rinse is a bit cleaner, and it gets counterflowed to become the first rinse of the next cycle. The final rinse is a fresh water fill, and after use it gets pumped back to become the second rinse in the next cycle.”

Probasco says equipment on the new line was optimized to minimize energy and water use while enabling the line to cover plating needs for a range of customer products. “To save energy, we can turn off sections of the line that we’re not using,” he says. “Rectifiers are sized to what we need here—they’re not 100-A rectifiers. The type and size of the anodes, the anode bags… everything was taken into consideration.”

Precision will also be translating this emphasis on flexible automation to the reel-to-reel portion of its business. The Belmontis know that such continuous evolution is one of the keys to survival in their niche of the plating industry. “Companies that do what we do fight pretty hard,” Gary Belmonti says. “Plating’s not an easy industry. As the landscape changes, becomes more and more competitive, there are fewer players that are left standing. We’re among some pretty fierce and knowledgeable competitors, and the bar just keeps getting raised.”



Zones | Suppliers | Products | Articles | Forums | Events | Clinics | Subscribe | Advertise | Contact Us

Products Finishing Magazine. The Web Resource For Product Finishing Professionals
®2008 Gardner Publications, Inc