Squeezing Money from Your Waste

Seneca Platers experienced an 82% reduction in weight and a 93% reduction in volume in one-tenth the time...

Racking Up a Success Story

Steel King installed a powder coating system and realized many benefits...

Assuring Paint Color at Behr

Spectrophotometer helps Behr monitor and control color consistency of its products . . .

Success
Ralph Waldo Emerson created a wonderful definition of success. "To laugh often and much; to win the respect of intelligent people and affection of children; to earn the appreciation of honest critics and endure the betrayal of false friends; to appreciate beauty, to find the best in others; to leave the world a bit better, whether by a healthy child, a garden patch or a redeemed social condition; to know even one life has breathed easier because you have lived.

New Generation Connector Finish

AMP develops a high-performance finish for its connector contacts...

Article Archive for: January 1999

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved