August 1996 ISSUE
COVER STORY
Converting from Leaded to Unleaded Electrocoat Primer
The customer wanted it and Thyssen delivered...
FEATURES
ElectroplatingAmerica's Oldest Gun Maker Adds a New Line
New black oxide line provides more than just a pretty finish...
Liquid Coating
Collecting Data Within an Electrocoating Tank
Submersible data acquisition unit measures voltage and current at specific areas on the part...
Electrocoating
Converting from Leaded to Unleaded Electrocoat Primer
The customer wanted it and Thyssen delivered...
Electroplating
Ion-Exchange Primer
A guide to understanding the basic principles of ion exchange...
Electroplating
Recycling/Recovery of Brass and Nickel
Not only does Thomas Industries recover brass and nickel, it recycles a lot of water too...