Rollomatic will display its ShapeSmart NP5 five-axis pinch and peel grinding machine for the cylindrical grinding of carbide, HSS and stainless steel components.

CLICK IMAGE TO ENLARGE (+)

Rollomatic will display its ShapeSmart NP5 five-axis pinch and peel grinding machine for the cylindrical grinding of carbide, HSS and stainless steel components. The machine provides high concentricity even on long and thin parts, the company says. Rough and finish grinding are performed in one pass using the peel grinding method, eliminating a separate process and reducing cycle time.
 
The Rollomatic GrindSmart 628XS six-axis tool and insert grinder with updated software will also be showcased.