Two visions of 3-D printing in CFRP

By: Ginger Gardiner
5. February 2014

Freespace Composites rendering and Mark One prototype 3-D carbon fiber printers.
Source: Freespace Composites and MarkForged

Both of these systems use carbon fiber in a thermoplastic matrix. Canada-based Freespace Composites is pursuing funding and finishing up software development. MarkForged (Cambridge, Mass.) has announced its Mark One is available for pre-order ($4,999) with shipments reported to start second half of 2014.

Freespace Composites employs a proprietary process that uses a high-strength carbon fiber-reinforced thermoplastic filament, placed optimally and continuously to produce continuous fiber structures in any direction. “Our printer consists of several multi-axis print mechanisms that are essentially 6-axis robot arms," says project principle, Nathan Armstrong. "Another 4-axis robot arm holds the part being printed, allowing the fiber to be placed in any direction, limited only by gravity and the physical possibilities of placement."

The design process starts in a standard structural optimization software package with available working volume and performance parameters as the only inputs. “However,” says Armstrong, “because our system is aimed at structural parts — nonstructural parts can be made with a normal layered printer — we are pushing linking the Freespace system directly to optimization-driven design.” This means optimization results are fed into proprietary “feedback loop” software that iteratively calculates part optimization vs. possible physical fiber placement. “Once this is complete,” explains Armstrong, “the 3-D printing process begins. This eliminates the traditional process of design/engineering/FEA/tooling by connecting optimization software directly to the 3-D printer.”

He describes the rendering above as a small industrial unit with a roughly 1m3 print area and adds, “we're exploring much larger print areas which use the same software but a much larger printer.” Armstrong and team are exploring partnerships for rollout and envision commercialization within five years.

MarkForged unveiled the Mark One — touted as the “World’s first carbon fiber 3-D printer” — at the SolidWorks World 2014 conference (Jan. 26-29, San Diego, Calif., USA). CEO Gregory Mark is an aerospace engineer whose previous company, Aeromotions, designs and builds computer-controlled carbon fiber composite race car wings. His vision was to use 3-D printing hardware to automate composite layup.


 

The Mark One’s specifications list poly lactic acid (PLA), nylon, continuous carbon and continuous glass filament as print materials and composite filament fabrication (CFF) and fused filament fabrication (FFF) as print techniques. The latter is another name for fused deposition modeling (FDM), while CFF is apparently Greg Mark’s creation. 3-D industry sources say it’s basically an extrusion printer, pushing 1.75 mm/0.07 inch FFF filament and 4 mm/0.2 inch CFF filament materials out through a dual extrusion head. Build volume is 305 by 160 by 160 mm (12 by 6.25 by 6.25 inches, or 486 in3).

Carbon fiber/nylon part in the Mark One 3-D printer. SOURCE: MarkForged

In his SolidWorks World presentation, Greg Mark said it took 20 design iterations to finalize the machining platform, or bed, which uses kinematic couplings (fixtures designed to constrain an object in place) to ensure the bed is within 10 microns of level every time it clicks into place.

The Mark One definitely benefits from slick industrial design and equally slick marketing. With its release going viral in the 3-D community, it will be interesting to see if the Mark One ‘greases’ development of novel composite structures.

Comments are reviewed by moderators before they appear to ensure they meet Products Finishing’s submission guidelines.
blog comments powered by Disqus

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2017

Subscribe | Advertise | Contact Us | All Rights Reserved