New global environmental directives are quickly moving the decorative coatings industry away from common hexavalent chrome technologies and into alternative trivalent chrome technologies. Understanding these directives, their impacts and technology options are imperative for finishers and manufacturers alike. This webinar will include an in depth review of EU REAcH Annex XIV, which mandates the elimination of decorative hexavalent chrome by September 21st, 2017 by all manufactures who supply into the EU and globally. Specific trivalent chrome alternatives will be reviewed in terms of their proposed capabilities along with the associated manufacturing realities for producers and finishers.