Rodger Talbert has been working in coatings and metal fabrication for more than 37 years. He has worked for a custom coater as vice president of sales and marketing, a company that designs and builds coating systems as a senior sales engineer and he ran his own consulting firm for over 18 years. He was the technical director and executive director of The Powder Coating Institute (PCI) from 2009 until 2012, when he took a position with TCI Powder Coatings as the company’s field technical director.

Have a question for Rodger? Send him an email.

 

The latest from the Powder Coating Clinic

Powder Coating Clinic: How to Stop Rust

Q. We make automated pay stations for parking lots, the machines that allow the customer to pay at the exit with a credit card or cash. We have had some problems with rust breaking out of the seams at the base and around the door panels that provide access to the interior of the machine. The machine works fine but customers are not happy with visible rust. We have tried to apply more coating but it will not penetrate the tight creases in these areas. We also have rust on the edges of the door frame and the door. What can we do to avoid this problem?

Ask an Expert Published: January 01, 2017

Powder Coating Clinic: Corrosion-Sensitive Environment

Q. I have some fencing around my swimming pool that has corroded badly over the years. It was made with steel and there is a lot of visible rust on the rails and vertical pickets. I am considering the options; have a professional painter come in and clean, repair and repaint the fence; or have the fence replaced with one better equipped to handle the harsh environment around the pool. What would you do if you were me?

Ask an Expert Published: January 01, 2017

Powder Coating Clinic: Adhesion Problems on Chromated Zinc Plating

Q. We have had adhesion issues when powder coating over zinc-plated aluminum. The aluminum had been nickel-flashed and zinc-plated with a hex-free chromate to meet RoHS compliance. Do you have any suggestions as to why the powder will not adhere properly to this surface?

Ask an Expert Published: January 01, 2017

Powder Coating Clinic: Solving Problems with Color Variation

Q. We are noticing differences in the color of parts coming out of the oven. It seems to happen more on some days than others. It can happen with any of our brighter colors like orange and red but does not seem to happen with more neutral colors like tan or gray. We use some infrared heaters in the first 20 feet of the oven and the rest is convection heating. We worked on balancing the oven but it is hard to get it level all the way through. What can cause color variation from part to part? How can we balance the oven and stop this problem?

Ask an Expert Published: December 01, 2016

Powder Coating Clinic: Oil Seeping out of Large Welded Tubing

Q. We have a large part made out of tubing that is welded together. The tubing has a lot of oil seeping out of the welds when the part is heated and causes a defect in the cured film. We cannot get the oil out of the tubing in our washer. We tried cleaning up the defect and running it again, but oil still runs out. How can we get that oil out of the tubing?

Ask an Expert Published: December 01, 2016

Powder Coating Clinic: Touch-up Options for Powder Coated Parts

Q. I’ve been told that a powder coated part cannot be “touched-up.” I have some patio furniture that I had powder coated and the powder coating shop that did the work for me stripped the threads in holes used to rack the part. I can fix the threads by welding up the hole and re-taping the threads. The shop states the whole piece will need to be redone and they cannot address just the small area affected by the repair. Is this accurate? Is it true that powder coating cannot be touched up?

Ask an Expert Published: December 01, 2016

Powder Coating Clinic: Powder in Layers

Q. We are in the process of designing a new powder system for aluminum extrusions and building panels. Our current system uses a six-stage dip pretreatment process and a three-layer liquid paint process (prime, color coat, clear coat) that meets AAMA 2605 standards (American Architectural Manufacturers Association). What layers of coating should we use and can we can meet the AAMA 2605 standards with powder?

Ask an Expert Published: December 01, 2016

Powder Coating Clinic: Making Powder Lines More Profitable

Q. We run a job shop powder coating operation with a conveyor system that runs at around 4 to 6 fpm, depending on what product is hung. We are putting through a lot of work, but our profits are not great. Can you suggest how to improve the efficiency, or cut our cost for a better profit margin? We cannot speed up the line because we do not have enough time in the cure oven to go faster. Our powder material cost seems to be higher than what we expect based on our quotes. What are we missing?

Ask an Expert Published: December 01, 2016

Powder Coating Clinic: Avoiding Rust on Parts

Q. We apply lighter colors of powder to our ticket machines for parking lots. Some go into covered garages, but many of them are exposed to the outdoor elements. We have some problems with rust around the base of the machines and also on corners. We currently run the steel parts through a five-stage iron phosphate washer, then apply a coat of TGIC polyester powder to a thickness of around 3 or 4 mils. What else should we be doing to prevent rust?

Ask an Expert Published: November 01, 2016

Powder Coating Clinic: Masking for Logo Design

Q. We are powder coating stainless steel water bottles for our company. For our logo, we would like to use a vinyl sticker or decal before powder coating. After the coating is applied, we want to peel the vinyl off to achieve a stainless steel logo effect, so we need some kind of temperature-resistant vinyl. Any suggestions?

Ask an Expert Published: November 01, 2016

Powder Coating Clinic: Discoloration of Metal-Flake in Powder

Q. We have a metal-flake silver powder color that we use regularly. If the surface is abraded with a Taber wheel—or even a pencil eraser—it darkens significantly in the abraded area. We even have this problem when our parts scrape against cardboard packaging. Our supplier suggested we switch from an unbonded leafing aluminum to a more expensive bonded product. We tried the bonded leafing aluminum, but we still have the same problem. Certain types of friction create this effect, seemingly those that perhaps have a higher coefficient of friction. Do they remove the aluminum flake from the surface? Can you explain this problem and tell us why it happens with some abrasives and not with others? What can we do to stop this? 

Ask an Expert Published: November 01, 2016

Powder Coating Clinic: Measuring Film Thickness before Cure

Q. How can I tell if the powder film build is thick enough before I cure the powder coating? We coat a lot of square footage and we need to control our cost. We often put on too much powder to avoid light coating. I need to know what my uncured film thickness is.

Ask an Expert Published: November 01, 2016

Enter your Message

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2016

Subscribe | Advertise | Contact Us | All Rights Reserved