Atotech Holds POP Summit for Customers

Atotech held its second Plating on Plastics (POP) summit in Rock Hill, South Carolina, on April 15.

Related Suppliers

Atotech held its second Plating on Plastics (POP) summit in Rock Hill, South Carolina, on April 15. The company provided several technical presentations on POP and decorative plating and introduced its new Cr(VI)-free etch technology, which Atotech says has already been successfully qualified under production scale conditions in the plating line at the Atotech TechCenters in Berlin, Germany. For more information, please visit Atotech.com.