Coventya Zinc Technology Meets GM Spec

News From: Products Finishing,

Posted on: 7/15/2013

Coventya’s Performatec P2260B zinc technology has been approved to General Motors' GMW 3044 Code X specification. Covered products include Zetaplus Merit, Lanthane TR-175 and FiniGard 460E.

Coventya’s Performatec P2260B zinc technology has been approved to General Motors' GMW 3044 Code X specification. Covered products include Zetaplus Merit, Lanthane TR-175 and FiniGard 460E.