Fiat Chrysler Automotive Approves Use of SWD’s Coating System

The PS-11036 coating system uses a zinc flake basecoat plus topcoat for corrosion protection.

Related Topics:

Fiat Chrysler Automotive (FCA; London, U.K.) has granted full approval to process parts in accordance with PS-11036 with a coating system from SWD Inc. (Addison, Illinois). SWD will apply a coating system using a zinc flake basecoat plus topcoat that provides good corrosion protection and consistent assembly torque.

The zinc-rich coating systems used at SWD are chromium-free as well as RoHS- and ELV-compliant. In addition to the new FCA PS-11036 coating, the company offers numerous automotive and industrial specifications including Honda HES-8000, GM 3359, CAT 1E1675G and Ford S-442. 

SWD Inc., 630 543-3003 or visit swdinc.com.