Formal Training Hours Per Employee Per Year

When it comes to formal training, more than 40 percent of employees get between 8-20 hours of training each year, the largest category in the Products Finishing Top Shops Benchmarking Survey for 2017 among electroplaters.

Related Topics:

When it comes to formal training, more than 40 percent of employees get between 8-20 hours of training each year, the largest category in the Products Finishing Top Shops Benchmarking Survey for 2017 among electroplaters. Second place was 21-40 hours at 27 percent, and then less than 8 hours annually came in at 23 percent. Just over 9 percent of respondents said their employees get over 40 hours of training annually.