PPG Industries’ industrial coatings business has raised prices an average of 5-10% on all its products in North America, a hike that when into effect Dec. 1, 2010.
“While PPG continues to implement cost-control measures throughout its operations, these efforts have not sufficiently offset rapidly rising raw material costs from key suppliers to the industrial coatings business, who are experiencing growing global demand as well as supply chain issues,” says Richard Zoulek, PPG general manager, industrial coatings, United States and Canada.