PPG Chromate-Free Primer, Pretreatment Standard on Boeing 737s

News Item From: Products Finishing

Posted on: 3/23/2012

Two chromate-free products from PPG Industries’ aerospace coatings group, a metal pretreatment and an exterior decorative primer, are now standard on Boeing Next-Generation 737 production airplanes.

Two chromate-free products from PPG Industries’ aerospace coatings group, a metal pretreatment and an exterior decorative primer, are now standard on Boeing Next-Generation 737 production airplanes. Desogel EAP-9 metal pretreatment and Desoprime CF/CA 7502 epoxy primer can be used with virtually any qualified topcoats.

According to PPG, the primer is the only chromate-free primer on Boeing’s qualified product list for its BMS 10-72 (revision Y) exterior decorative paint specification, and airlines also are requesting the product with a non-chromated pretreatment for Boeing 767 and 777 widebodies. 


Learn More

Related Suppliers

PPG

Zones

Supplier Categories


Global Finishing Solutions
Kremlin by EXEL North America

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved