PPG Industries’ industrial coatings business has created a dedicated electronic materials group to integrate products and technologies it acquired from Spraylat Corp. in December.

Related Suppliers

PPG Industries’ industrial coatings business has created a dedicated electronic materials group to integrate products and technologies it acquired from Spraylat Corp. in December. The company now offers a full line of electrically conductive, resistive and dielectric inks and conductive coatings for radio-frequency interference/electromagnetic interference (RFI/EMI) suppression.

These inks and coatings are used in such applications as touch-control panels for smartphones, tablets and other consumer devices; interactive and electrochromic displays; biomedical sensors; printed keypads and other industrial membrane switch controls; radio-frequency identification tags; and other products that require printed circuitry.