PPG Industries’ industrial coatings business has awarded Astro Shapes Inc. premier member accreditation in its PPG Certified Applicator Program (PPG/CAP). This enables the Struthers, Ohio, commercial coater to apply PPG’s Duranar powder coatings to aluminum architectural components. The PPG/CAP guidelines establish protocols to help minimize color variance across the components.