PPG Publishes Data Sheets for UL-Recognized Components

The data sheets cover PPG brands and resin chemistries for liquid, powder, electrocoat products.

Related Suppliers

PPG Industries (Pittsburgh, Pennsylvania) has published three data sheets documenting PPG coating systems recognized under the Component Recognition Program of Underwriters Laboratories (UL) for the UL 1332 Standard for organic coatings. The three data sheets cover liquid, powder and electrocoat products individually and list brands, resin chemistries and coating systems for each technology that are UL-recognized components under Standard UL 1332. The data sheets also detail the pretreatment systems and substrates for which the recognition is valid. Maria Lamorey, PPG business development manager, electrical transmission and distribution equipment, says the data sheets enable PPG to provide electrical equipment manufacturers with printed documentation for its systems recognized under the Component Recognition Program of UL.