Bonderite NT is a  nanotechnology-based conversion coating for metals and is said to be free of phosphate and toxic heavy metals, to be ultra thin, uniform and make production process economical. This coating is suitable for surface pretreatment for conventional powder and wet paint coatings. It can be applied by dipping or spraying and creates a cohesive, inorganic, high-density layer incorporating nanoparticles. The process has low energy needs (saving money) and is also distinguished by its entire lack of organic ingredients.