E-Brite Ultra Cu is a unique cyanide-free alkaline copper plating process with covering and throwing powers greater than cyanide copper. The process plates on steel, zinc diecast, zincated aluminum,brass, electroless nickel, and watts nickel.

The process is an excellent pre-plate copper strike for bright nickel, acid copper, tin and solder plates.  It is an excellent heat treat stop off plate and EMI shield. It is also an excellent decorative finish for buttons, rivets, lighting fixtures and builders’ hardware. The copper plate can be readily blackened or oxidized for a variety of attractive antiqued finishes.

It is said to have no carbonates that need to be treated nor contain strong chelators. It is supplied as a liquid concentrate which is diluted with water.

The plating process produces a fine grained, smooth, dense and ductile copper deposit which is nonporous and has excellent bonding properties. It is designed to be the next generation process to E-Brite 30/30 process and works in rack or barrel processes.

 

PF Direct
EPi - Electrochemical Products
17000 W. Lincoln Ave
New Berlin, WI 53151
Phone (262) 786-9330 Fax (262) 786-9403



Zones | Suppliers | Products | Articles | Forums | Events | Clinics | Subscribe | Advertise | Contact Us

Products Finishing Magazine. The Web Resource For Product Finishing Professionals
®2008 Gardner Publications, Inc