ENTHOBRITE CLZ-970 bright acid zinc plating process provides the high productivity of a water-soluble process while maintaining superior distribution and deposit properties at any chloride level. According to the manufacturer, this results in a substantial increase in productivity and a dramatic decrease in zinc plating costs. The process, featuring a high-temperature tolerance that can operate as a potassium chloride, ammonium chloride or mixed system, is designed to deliver improved plate distribution and optimized metal efficiency, and is specially formulated for continuous, high throughput operations. It also possesses a high cloud point that will not decline over time due to additive breakdown products.