The PosiTestR pull-off adhesion tester measures adhesion of coatings to metal, masonry and other substrates.

The PosiTestR pull-off adhesion tester measures adhesion of coatings to metal, masonry and other substrates. It measures the force required to pull a specified test diameter of coating away from its substrate using hydraulic pressure. The pressure is displayed in both MPa and psi on a precision dial indicator and can be related to the strength of adhesion to the substrate.