AkzoNobel Powder Coatings has expanded the warranty system for its Interpon D line of AAMA-compliant architectural powder coatings, which includes a range of products to comply with AAMA 2603, 2604 and 2605 in a variety of colors and effects.

Related Topics:

Related Suppliers

AkzoNobel Powder Coatings has expanded the warranty system for its Interpon D line of AAMA-compliant architectural powder coatings, which includes a range of products to comply with AAMA 2603, 2604 and 2605 in a variety of colors and effects.

Interpon D1010 series products comply with AAMA 2603 and come with a 10-year warranty. Interpon D 2000 series products are AAMA 2604-compliant and come with a 20-year warranty; and Interpon D3000 series products are AAMA 2605-compliant and come with a 30-year warranty.

Editor Pick

O&S Expo Renamed as “SurfaceTechnology GERMANY”

Global trade fair organizer Deutsche Messe AG announces renaming its surface finishing O&S Expo to “SurfaceTechnology GERMANY.” The new name is already in effect for the next edition of the international trade fair for surface treatment technology from June 5 to 8 this year in Stuttgart, Germany.