Aqueous Cleaner for Copper Alloys

Kyzen will highlight its Metalnox M6310 cleaning chemistry designed for heavy-duty cleaning of dry lube, cutting, oils, waxes, grease, carbonized soils and shop dirt.

Related Suppliers

Kyzen will highlight its Metalnox M6310 cleaning chemistry designed for heavy-duty cleaning of dry lube, cutting, oils, waxes, grease, carbonized soils and shop dirt. The mild-alkaline aqueous cleaner is multi-metal safe and contains no amines. Designed for brass screw machine parts, the chemistry contains corrosion inhibitors for aluminum, brass and other copper alloys. The cleaner can also be used with tungsten carbide, die cast aluminum and other metals that are susceptible to chemical attack, the company says.