The company's Multi-MasksTM serve as both a cap and a tapered plug.

The company's Multi-MasksTM serve as both a cap and a tapered plug. While being capable of masking studs or tube ends, they are also used for threaded and blind holes. This product is said to be ideal for job shop coating services that need a variety of functions from one item.  Designed to be used for powder coating, e-coating, plating and anodizing, they are color coded for easy sorting and are reusable. Custom sizes are available by special order with little or no setup fees.