Technic Inc. has released a new cyanide-free silver-plating process chemistry—Cy-less II-W.

Technic Inc. has released a new cyanide-free silver-plating process chemistry—Cy-less II-W. Designed for the general metal finishing, decorative and electronic component/connector applications, Cy-less II-W addresses the demand for an environmentally-safe high-performance silver process. What makes Cy-less II-W a significant addition to Technic’s existing line of cyanide free products is its bright, non-yellow appearance and even distribution.