Okuno Chemical will demonstrate its CRP process for direct-acid copper plating on plastics, which the company says offers reduces environmental loads wastewater treatment costs. It also will highlight its electroless nickel and anodizing processes.

Okuno Chemical will demonstrate its CRP process for direct-acid copper plating on plastics, which the company says offers reduces environmental loads wastewater treatment costs. It also will highlight its electroless nickel and anodizing processes. 