Coventya’s Enova EF electroless nickel coatings are free from lead or cadmium, offering wear resistance and corrosion protection while meeting RoHS and ELV directives.

CLICK IMAGE TO ENLARGE (+)

Coventya’s Enova EF electroless nickel coatings are free from lead or cadmium, offering wear resistance and corrosion protection while meeting RoHS and ELV directives.

The coatings provide consistent deposition and are versatile under a variety of production conditions, the company says. They are designed for increased solution life and stability, especially on nonferrous substrates, brass and copper alloys. 


Learn More

Related Suppliers

COVENTYA Inc.

Zones

Supplier Categories


Loading the player ...
Technic Inc
Pavco
Insoluble Anodes
Luster-On Products

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved