Escomatic Wire Company Offers New Brass and Stainless Steel Grades

Niche market distributor Metal Resource Solutions Inc. (MRSI) offers new sizes and material grades to its escomatic wire stocking program.

Niche market distributor Metal Resource Solutions Inc. (MRSI) offers new sizes and material grades to its escomatic wire stocking program. It offers CDA 360 and CDA 353 brass as well as stainless steel grades 303 & 416 escomatic quality wire in diameters ranging from 0.0625” up to 0.3125”.

This benefits customers by offering one-stop shopping for commonly used grades and sizes in brass and stainless steel. According to the company, feedback regarding its program has been very positive; it has received high marks for quality, packaging, value and customer service.