Flexible Hose Replaces PVC, Rubber for Pneumatic Conveying

New Product Announcements From: Products Finishing

Posted on: 1/11/2012

Flexaust’s FlexStat 60 static dissipative polyurethane hose is heavy-walled, but flexible, and designed to replace PVC and rubber hose in demanding bulk pneumatic conveying applications.

CLICK IMAGE TO ENLARGE (+)

Flexaust’s FlexStat 60 static dissipative polyurethane hose is heavy-walled, but flexible, and designed to replace PVC and rubber hose in demanding bulk pneumatic conveying applications. The hose features a 0.06-inch-thick wall reinforced with a rigid, external ABS helix, and an embedded copper grounding wire. A smooth interior minimizes friction loss.

The hose is available with 4-, 5-, 6- and 8-inch IDs, and in lengths of 25 and 50 ft. It exhibits 108–1,010 ohms/square surface resistivity and operates from -40°F to 200°F. 


Learn More

Zones

Supplier Categories


Finishing Equipment
Col-Met
Magic Rack
Finishing Solutions
SIDSP
Therma-Tron-X

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved