720&722 This company wil feature its Duraseal Plus, which is a liquid sealer applied over chromated electrodeposited zinc.

720&722

This company wil feature its Duraseal Plus, which is a liquid sealer applied over chromated electrodeposited zinc. The product claims to increase salt spray performance to white corrosion to 120 hours for conventional trivalent blue-bright chromates, and more than 200 hours for higher performing chromates. Duraseal Plus Yellow creates yellow irridescence over topcoating when added to the bath.