Inorganic Coating Replaces Phosphates in Pretreating Metal

New Product Announcements From: Products Finishing

Posted on: 8/15/2011

Bulk Chemicals’ Zirca-Sil is a homogeneous inorganic coating designed to replace traditional iron and zinc phosphates as a metal pretreatment.

Bulk Chemicals’ Zirca-Sil is a homogeneous inorganic coating designed to replace traditional iron and zinc phosphates as a metal pretreatment. The coating forms a thin layer of a nano/metallic matrix as a protective film on metal surfaces. Performance is equal to traditional phosphates, the company says. 


Learn More

Editor's Picks

NAI Coating Show 2011

NACE International and the Powder Coating Institute host the 2011 NAICS in Cincinnati, Ohi...

Related Suppliers

Bulk Chemicals, Inc. - BCI Surface Technologies

Zones

Supplier Categories


Loading the player ...
Insoluble Anodes
Pavco
Technic Inc
Luster-On Products

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved