Internal Pipe Coatings Offer Chemical Resistance in High Temperatures

New Product From: Products Finishing, from Products Finishing

Posted on: 12/8/2016

Axalta Coating Systems introduces two new high-temperature, corrosion-resistant internal pipe coatings to its Nap-Gard Functional Coatings collection.

CLICK IMAGE TO ENLARGE (+)

 

Axalta Coating Systems introduces two new high-temperature, corrosion-resistant internal pipe coatings to its Nap-Gard Functional Coatings collection. The new Nap-Gard 7-0017HT and 7-0017VHT Black Beauty FBE products are thermosetting epoxy powders designed to provide chemical resistance when operating in temperatures up to 392°F (200°C).

According to the company, corrosion caused by carbon dioxide (CO2) and hydrogen sulfide (H2S), often found in sour crude oil, is a major challenge for oil and gas industry. Axalta’s introduction of these high glass transition (Tg) temperature internal pipe coatings are designed to combat this problem. When properly applied with Nap-Gard 7-1808 primer, Nap-Gard 7-0017HT and 7-0017VHT can offer corrosion protection against high levels of H2S and CO2, as well as methane (CH4), even at high temperatures and pressures.

The Nap-Gard collection of powder coatings is used on external and internal oil, gas and water pipelines with single, dual, and multi-layer application options. Nap-Gard also provides corrosion protection solutions used to coat valves, fittings and rebar.

For more information, visit axaltacs.com/powder.

 

 

Comments are reviewed by moderators before they appear to ensure they meet Products Finishing’s submission guidelines.
blog comments powered by Disqus


Learn More

Related Suppliers

Axalta Coating Systems

Zones


SIDSP
Therma-Tron-X
Magic Rack

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2016

Subscribe | Advertise | Contact Us | All Rights Reserved