IGP North America LLC offers its IGP-RAPIDcomplete ultra-low-curing, polyester-resin-based powder coating system for use on medium-density fiberboard (MDF) and other temperature-sensitive substrates.

Related Topics:

IGP North America LLC offers its IGP-RAPIDcomplete ultra-low-curing, polyester-resin-based powder coating system for use on medium-density fiberboard (MDF) and other temperature-sensitive substrates. Designed for finishing applications in the furniture, kitchen cabinet and general finishing markets, the coating system provides a high-quality finish while curing in 3 min. at temperatures as low as 250°F, according to the company. Required substrate preheat temperature is as low as 120°F.

According to the company, this coating enables finishing with only one coat, increasing throughput by as much as 50 percent. Available in a range of solid colors as well as smooth, semi-smooth and texture finishes, this coating meets or exceeds some of the Kitchen Cabinet Manufacturing Association (KCMA) and American National Standards Institute (ANSI) standards as well other manufacturer performance specifications.

IGP North America LLC, call 502 939 5606 or visit igp.ch/en.