Metal Pretreatment System Passivates, Seals Without Rinse

Chemtec North America will showcase Toran 3/P, a metal pretreatment system designed to passivate and seal metal surfaces in a single step without a rinse stage.

Related Topics:

Chemtec North America will showcase Toran 3/P, a metal pretreatment system designed to passivate and seal metal surfaces in a single step without a rinse stage. The system cures at room temperature and is said to offer enhanced flash rust protection before topcoating and corrosion resistance when used with topcoats. According to the company, the system uses no water, and creates no liquid or solid waste.