Mid America Alloys

912 Zinc anodes products are offered in a variety of shapes and sizes.

Related Topics:

912

Zinc anodes products are offered in a variety of shapes and sizes. Some electroplating grade zinc anodes are offered in ingot form. Drilled and tapped anodes are made to order and other specialty sizes and shapes are available. Other zinc products are available from zinc alloys for the zinc die casting industry, to sacrificial anodes made from special high-grade zinc for the corrosion control industry. 