Nalco Corporation will be presenting its Tech Bond® Sol-Gel Nanotechnology, a new, patented, treatment for aluminum that is chrome-free, is said to have unmatched corrosion resistance properties and maintains the natural aesthetics of aluminum.

Related Topics:

Nalco Corporation will be presenting its Tech Bond® Sol-Gel Nanotechnology, a new, patented, treatment for aluminum that is chrome-free, is said to have unmatched corrosion resistance properties and maintains the natural aesthetics of aluminum.  Testing is said to have prove that Tech Bond products can exceed industry standards for the corrosion protection and paint performance of aluminum surfaces, while reducing total operating costs.  Company scientists have formulated this revolutionary technology to work with the natural properties of aluminum, making it the most effective corrosion protection per unit thickness ever invented. 

 

Tech Bond nanocoating has numerous benefits including simple application, colorless formulation, and a metals-free composition that makes it extremely safe to prepare and use.  It does not contain any phosphates and is ELV, RoHS and WEEE compliant.  And, the simple application process reduces production time and eliminates extra chemical costs that come from processing ingredients.