Eco-Tec’s NickelPur nickel recovery system uses Recoflo ion-exchange technology with compressed beds and counter-current regeneration to recover nickel dragged out from plating baths into the rinses.

Related Suppliers

Eco-Tec’s NickelPur nickel recovery system uses Recoflo ion-exchange technology with compressed beds and counter-current regeneration to recover nickel dragged out from plating baths into the rinses. Cation exchange and acid sorption beds are coupled to produce a concentrated de-acidified nickel salt product. Rinse water is pumped through cartridge filters and then through the strong acid cation resin bed where the nickel is exchanged on the resin.