Uni-Spray will introduce its new Green Technology Nozzles at Fabtech. The nozzles offer the same performance as the company’s standard products, yet leave no carbon footprint. Traditional plastic nozzles will survive for 100-plus years in a landfill. Due to a special additive, the Green Technology Nozzles will completely break down in 1 to 3 years, the company says.