OMG Electronic Chemicals introduces OMG Fidelity’s 9159, a 100% lead and cadmium free, full bright, medium phosphorous, self pH regulating electroless nickel bath. RoHS compliant 9159 is a stable, robust bath that maintains brightness and rate throughout its bath life. 9159 is appropriate for automotive, electronic and general metal finishing applications
OMG is a vertically integrated, global leader in the production of metal based specialty chemicals and associated products. OMG Electronic Chemicals is a leading global supplier of metal based specialty chemicals for surface finishing. OMG Fidelity’s 9159 is a bath unique to the market, designed to meet the need for a self-pH regulating, bright LFCF MPEN.