Wisconsin Oven designed and manufactured a gas fired conveyor oven with a blow off and cool down for drying moisture on aluminum replacement coils.
Wisconsin Oven designed and manufactured a gas fired conveyor oven with a blow off and cool down for drying moisture on aluminum replacement coils. The oven has horizontal airflow and a 300º F maximum operating temperature.
Prior to entering the oven, the aluminum replacement coils are leak tested. The coils are then processed through the drying system at a rate of 60 units per hour. After exiting the oven, the coils go directly to packaging. A systems acceptance test that required the end product to only weigh .16 oz more than the pre-water bath passed on all 30 parts tested.