Pavco is pleased to present its broad line of alloy products to meet the demands of the fast growing market for automotive. Volta is a sulfate based tin-zinc electroplating process that produces a tin/zinc alloy containing 70% tin and 30% zinc. Niclipse is an acid zinc/nickel plating process that achieves 12-15% nickel in the deposit, while offering exceptional corrosion resistance and demonstrating superior metal distribution and covering power. Finally, Ziniloy is an alkaline zinc-nickel plating process that deposits 12-15% nickel in the deposit and offers 30% more efficiency than conventional processes.