The Decoral® system is said to be a simple and elegant process that can give aluminum components a highly decorative and individual surface finish.

The Decoral® system is said to be a simple and elegant process that can give aluminum components a highly decorative and individual surface finish. The system is a special powder coating formulated with raw materials and is applied on aluminum and polymerized as the first coat. The desired pattern is transferred from a pre-print film onto the coated component, which is heated againt for this purpose. The process offers designers virtually unlimited cope for decorating three-dimensional aluminum components with wood grain, marble, granite or fantasy effects.