Pamphlet describes pulse plating, its advantages and typical applications.

Pamphlet describes pulse plating, its advantages and typical applications. In pulse plating, DC power is supplied to the plating bath in a series of short pulese rather than by continuous current. Pulse Plating can provide a better overall finish, better distribution, lower porosity, higher density, better colo control, lower wear rates, less metal use, greater throwing power and improved hardness.