Turbo Spray's #2001S rotary-head HVLP gun is designed to spray liquid coatings (paints, adhesives, mold releases and slip coatings) into recessed and hidden areas on a variety of substrates. The gun’s extended, 360-degree air-cap-rotation capability enables users to spray recesses and side walls on ID-sprayed parts without requiring multiple guns to do the same process.
The gun can be mounted stationary on a reciprocator or on a robot. For robotic applications, it can spray from multiple angles using low atomizing and fluid pressure, reducing programming time and robot fatigue.