Rust and Scale Remover

Pico has engineered an environmentally-acceptable, user-friendly, pH-neutral cleaner concentrate in Picoclean X-Rust designed to remove rust and corrosion attack from metal surfaces safely, quickly and completely.

Related Suppliers

Pico has engineered an environmentally-acceptable, user-friendly, pH-neutral cleaner concentrate in Picoclean X-Rust designed to remove rust and corrosion attack from metal surfaces safely, quickly and completely. Other methods of rust removal have included harsh, corrosive chemicals or arduous physical brushing and blasting methods resulting in downgraded finished product, scrapped material and rejected shipments. Mixed at low dilution rates in water, Picoclean X-Rust is most often utilized in a room temperature soak application. Parts, pieces and products are restored to brand new condition, and an indiscernible, molecular layer of material left behind after use provides additional short-term protection.