rust preventative liquid

HALOX® 900 is a water-based, nitrite-free temporary corrosion inhibitor.

HALOX® 900 is a water-based, nitrite-free temporary corrosion inhibitor. It is formulated with a patented technological chemistry to offer corrosion protection for both ferrous and non-ferrous metals.  In addition to providing temporary rust protection to bare metal, it also promotes adhesion of coating to the substrate.

Proper use of inhibitor consists of diluting the product in water and then applying by immersion or spray.  The dilution levels are based on the degree of protection and the environment of exposure for bare metals.