Satin Finish Decorative Nickel Plating Process

New Product Announcements From: Products Finishing

Posted on: 4/1/2011

Coventya Inc.'s newest addition to its line of decorative nickel plating technologies is the Satin Crystal 230 Process.

CLICK IMAGE TO ENLARGE (+)

Satin Crystal 230

Satin Crystal 230

Coventya Inc.'s newest addition to its line of decorative nickel plating technologies is the Satin Crystal 230 Process. The distinguishing feature of the process is its ability to provide remarkably uniform white,-silver satin deposits at all current densities, even those corresponding to recessed areas on production parts, the company says.

The process is designed for installations that require flexibility in the satin appearance due to processing a variety of work, from exterior rand interior automotive trim, to furniture, plumbing and shelving.


Learn More

Related Suppliers

COVENTYA Inc.

Zones

Supplier Categories


Insoluble Anodes
Technic Inc
Luster-On Products
Pavco

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved