Dampney’s Endcor 8898 silicone-alkyd copolymer self-priming coating is designed for use on cast iron and steel surfaces requiring high gloss, color retention and weather resistance.

CLICK IMAGE TO ENLARGE (+)

Dampney’s Endcor 8898 silicone-alkyd copolymer self-priming coating is designed for use on cast iron and steel surfaces requiring high gloss, color retention and weather resistance. It is formulated to resist UV, chalking, fading, moisture and salt spray, is VOC-compliant and can be applied over solvent-cleaned surfaces using conventional airless spray or brush.

The coating is 60 percent solids by volume and resists 300°F continuous exposure. It is suited for utility meters, valves, and commercial and industrial equipment. According to the company, it has been approved by major utilities for electric- and water-meter and valve maintenance and manufacturing. 


Learn More

Related Suppliers

Dampney Company, Inc.

Zones

Supplier Categories


Kremlin by EXEL North America
Global Finishing Solutions

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved