Sherwin-Williams’ Water Reducible Enamel Delivers One-Coat Protection

This enamel is intended for industrial product finishing and refinishing applications and provides great corrosion resistance.

Related Topics:

Related Suppliers

With 30 minutes dry to touch, 75 minutes dry to handle and one-coat application, Sherwin-Williams’ Kem Aqua 8710 water reducible acrylic modified alkyd system increases throughput efficiency and also passes 100 hours salt spray at 1.2 DFT.  This enamel is intended for industrial product finishing and refinishing applications and provides great corrosion resistance. Kem Aqua 8710 offers good flexibility and mar resistance, and is offered in a broad range of colors and glosses.